粘土砖理化指标:
项目 |
指标 |
||||||||
N-1 |
N-2a |
N-2b |
N-3b |
N-4 |
N-5 |
N-6 |
|||
耐火度°C> |
1750 |
1730 |
1730 |
1710 |
1690 |
1670 |
1580 |
||
荷重软化开始温度≥ |
1400 |
1350 |
|
|
1300 |
|
|
||
重烧线变化% |
1400°C 2h |
0.1 |
0.1 |
0.2 |
|
|
|
|
|
-0.4 |
-0.5 |
-0.5 |
|
|
|
|
|||
1350° 2h |
|
|
|
0.2 |
0.2 |
0.2 |
|
||
|
|
|
-0.5 |
-0.5 |
-0.5 |
|
|||
显气孔率< |
22 |
24 |
26 |
24 |
24 |
26 |
28 |
||
常温耐压强度>MPa |
30 |
25 |
20 |
15 |
20 |
15 |
15 |
수입신고 1USD |
구매/결제대행 1CNY |
TT송금 1CNY |
---|---|---|
7.16 CNY | 193.76 KRW | 0.145 USD |